Lucas Labs Pro4
Apparatus |
| Pro4 |
Supplier | Lucas Labs https://signatone.com/manual-sheet-resistivity-measurement-system/ | |
Location | P.00.351 (TU14 1/2) | |
Function | 4 point probe measurement | |
Main purpose | measure sheet resistance of thin films | |
Main characteristics | ||
Facilities | 4 point probe head with Keithley 2400 source meter | |
Typical application | measure sheet resistance of thin films | |
Specimen | max. 4 inch | |
Equipment owner | Lodi Schriek +31 634321293
Roald v.d. Kolk (back-up) +31 634321301 |